高Cr马氏体耐热钢的协同强化机制及形变热处理应用 |
| 张竟文, 余黎明, 刘晨曦, 丁然, 刘永长 |
|
Synergistic Strengthening of High-Cr Martensitic Heat-Resistant Steel and Application of Thermo-Mechanical Treatments |
| ZHANG Jingwen, YU Liming, LIU Chenxi, DING Ran, LIU Yongchang |
| 图1 高Cr马氏体耐热钢微观组织特征[ |
| Fig.1 Microstructure characteristics and synergistic strengthening of the high-Cr martensitic heat-resistant steels (a) schematic diagram[ (b) synergistic strengthening of lath interfaces, dislocations, and precipitates |
|