微弧氧化时间对锆合金表面MAO/Cr复合涂层结构与性能的影响 |
| 王郑, 王振玉, 汪爱英, 杨巍, 柯培玲 |
|
Influence of Micro-Arc Oxidation Time on Structure and Properties of MAO/Cr Composite Coatings |
| WANG Zheng, WANG Zhenyu, WANG Aiying, YANG Wei, KE Peiling |
| 图9 MAO9min/Cr复合涂层在900℃水蒸气环境中的氧化过程示意图 |
| Fig.9 Schematic of oxidation process of the MAO9min/Cr composite coating on Zirlo substrate at 900oC in steam environment |
|