微弧氧化时间对锆合金表面MAO/Cr复合涂层结构与性能的影响 |
| 王郑, 王振玉, 汪爱英, 杨巍, 柯培玲 |
|
Influence of Micro-Arc Oxidation Time on Structure and Properties of MAO/Cr Composite Coatings |
| WANG Zheng, WANG Zhenyu, WANG Aiying, YANG Wei, KE Peiling |
| 图8 HF酸溶液刻蚀后3种腐蚀态复合涂层的截面形貌 |
| Fig.8 Cross-sectional morphologies of the three corrosive composite coatings etched by HF sloution (a) MAO3min/Cr (b) MAO6min/Cr (c) MAO9min/Cr |
|