微弧氧化时间对锆合金表面MAO/Cr复合涂层结构与性能的影响
王郑, 王振玉, 汪爱英, 杨巍, 柯培玲

Influence of Micro-Arc Oxidation Time on Structure and Properties of MAO/Cr Composite Coatings
WANG Zheng, WANG Zhenyu, WANG Aiying, YANG Wei, KE Peiling
图5 高温水蒸气腐蚀后3种复合涂层的氧化增重和物相组成及织构系数
Fig.5 Mass gain (a), XRD spectra (b), and texture coefficients (c) of the three composite coatings after high-temperature steam oxidation