微弧氧化时间对锆合金表面MAO/Cr复合涂层结构与性能的影响 |
| 王郑, 王振玉, 汪爱英, 杨巍, 柯培玲 |
|
Influence of Micro-Arc Oxidation Time on Structure and Properties of MAO/Cr Composite Coatings |
| WANG Zheng, WANG Zhenyu, WANG Aiying, YANG Wei, KE Peiling |
| 图4 纯Cr涂层和复合涂层的硬度曲线和相应的压痕形貌 |
| Fig.4 Hardness curve and corresponding indentation morphologies (insets) of Cr coating and MAO/Cr composite coatings |
|