微弧氧化时间对锆合金表面MAO/Cr复合涂层结构与性能的影响 |
| 王郑, 王振玉, 汪爱英, 杨巍, 柯培玲 |
|
Influence of Micro-Arc Oxidation Time on Structure and Properties of MAO/Cr Composite Coatings |
| WANG Zheng, WANG Zhenyu, WANG Aiying, YANG Wei, KE Peiling |
| 图3 3种复合涂层的表/截面形貌的SEM像 |
| Fig.3 Surface (a1, a2, b1, b2, c1, c2) and cross-sectional (a3, b3, c3) SEM images of the three composite coatings (a1-a3) MAO3min/Cr (b1-b3) MAO6min/Cr (c1-c3) MAO9min/Cr |
|