电弧微铸锻复合增材制造GH4169D高温合金的显微组织与力学性能 |
| 曾立, 王桂兰, 张海鸥, 翟文正, 张勇, 张明波 |
|
Microstructure and Mechanical Properties of GH4169D Superalloy Fabricated by Hybrid Arc and Micro-Rolling Additive Manufacturing |
| ZENG Li, WANG Guilan, ZHANG Haiou, ZHAI Wenzheng, ZHANG Yong, ZHANG Mingbo |
| 图12 HARAM工艺成形GH4169D合金经SA和HSA热处理后室温拉伸试样断口形貌的SEM像 |
| Fig.12 Fracture SEM images of HARAM-ed GH4169D superalloy after SA (a) and HSA (b) treatments |
|