Microstructure and Mechanical Properties of GH4169D Superalloy Fabricated by Hybrid Arc and Micro-Rolling Additive Manufacturing |
| ZENG Li, WANG Guilan, ZHANG Haiou, ZHAI Wenzheng, ZHANG Yong, ZHANG Mingbo |
| 图4 电弧熔丝增材制造(WAAM)和HARAM工艺成形的未热处理态GH4169D合金试块宏观形貌和微观组织的OM像 |
| Fig.4 Macrostructures (a, b) and OM images (c, d) of WAAM-ed (a, c) and HARAM-ed (b, d) GH4169D block samples (WAAM—wire and arc additive manufacturing) |
|