Zr-1Nb-xFe合金在模拟LOCA下的高温蒸汽氧化行为 |
| 王金鑫, 姚美意, 林雨晨, 陈刘涛, 高长源, 徐诗彤, 胡丽娟, 谢耀平, 周邦新 |
|
High Temperature Steam Oxidation Behavior of Zr-1Nb- xFe Alloy Under Simulated LOCA Condition |
| WANG Jinxin, YAO Meiyi, LIN Yuchen, CHEN Liutao, GAO Changyuan, XU Shitong, HU Lijuan, XIE Yaoping, ZHOU Bangxin |
| 图4 0Fe、0.05Fe、0.2Fe和0.4Fe合金在1000、1100和1200℃高温蒸汽中恒温3600 s后横截面的OM像 |
| Fig.4 Cross-sectional OM images of 0Fe (a1-a3), 0.05Fe (b1-b3), 0.2Fe (c1-c3), and 0.4Fe (d1-d3) alloys oxidized in 1000oC (a1-d1), 1100oC (a2-d2), and 1200oC (a3-d3) steam for 3600 s |
|