Zr-1Nb-xFe合金在模拟LOCA下的高温蒸汽氧化行为 |
| 王金鑫, 姚美意, 林雨晨, 陈刘涛, 高长源, 徐诗彤, 胡丽娟, 谢耀平, 周邦新 |
|
High Temperature Steam Oxidation Behavior of Zr-1Nb- xFe Alloy Under Simulated LOCA Condition |
| WANG Jinxin, YAO Meiyi, LIN Yuchen, CHEN Liutao, GAO Changyuan, XU Shitong, HU Lijuan, XIE Yaoping, ZHOU Bangxin |
| 图3 0Fe、0.05Fe、0.2Fe和0.4Fe合金在900℃高温蒸汽中恒温3600 s后横截面的OM像 |
| Fig.3 Cross-sectional OM images of 0Fe (a1, a2), 0.05Fe (b1, b2), 0.2Fe (c1, c2), and 0.4Fe (d1, d2) alloys oxidized in 900oC steam for 3600 s (Figs.3a2-d2 are the enlarged images of middle area of Figs.3a1-d1, respectively) |
|