基于熔池原位冶金的电弧增材制造Al-Cu-Li合金显微组织与硬度
黎康杰, 孙泽羽, 何蓓, 田象军

Microstructure and Hardness of Al-Cu-Li Alloy Fabricated by Arc Additive Manufacturing Based on In Situ Metallurgy of Molten Pool
LI Kangjie, SUN Zeyu, HE Bei, TIAN Xiangjun
表2 各种工艺下合金试样的Vickers硬度[11,24,25]
Table 2 Average Vickers hardnesses of the alloy samples under various processes[11,24,25]
ProcessMaterialStateVickers hardness / HV0.1Ref.
MIG2219 + Al-Li powderAs-build126.7 ± 2.1This work
TIG2219 + TiCAs-build97.5 ± 2.5[11]
TIG2219As-build89 ± 4[24]
Laser + TIG2219As-build92.6 ± 3.7[25]