V和B元素对Ti-44Al-5Nb-1Mo合金显微组织及热变形机制的影响 |
| 李天瑞, 许瑜倩, 吴文平, 甘文萱, 杨永, 刘国怀, 王昭东 |
|
Effects of V and B on the Microstructure Evolution and Deformation Mechanisms of Ti-44Al-5Nb-1Mo Alloys |
| LI Tianrui, XU Yuqian, WU Wenping, GAN Wenxuan, YANG Yong, LIU Guohuai, WANG Zhaodong |
| 图1 Ti-44Al-5Nb-1Mo和Ti-44Al-5Nb-1Mo-2V-0.2B合金均匀化后的SEM像 |
| Fig.1 Low (a, c) and high (b, d) magnified SEM images of as-homogenized Ti-44Al-5Nb-1Mo (a, b) and Ti-44Al-5Nb-1Mo-2V-0.2B (c, d) alloys |
|