预氧化处理对12Cr铁素体/马氏体钢耐Pb-Bi腐蚀性能的影响 |
| 潘霞, 张洋鹏, 董志宏, 陈胜虎, 姜海昌, 戎利建 |
|
Effect of Pre-Oxidation Treatment on the Corrosion Resistance in Stagnant Liquid Pb-Bi Eutectic of 12Cr Ferritic/Martensitic Steel |
| PAN Xia, ZHANG Yangpeng, DONG Zhihong, CHEN Shenghu, JIANG Haichang, RONG Lijian |
| 图9 未预氧化和预氧化处理的12Cr铁素体/马氏体钢样品经550℃饱和氧LBE腐蚀500 h后的表面SEM-BSE像 |
| Fig.9 SEM-BSE surface images of 12Cr ferritic/martensitic steel samples without (a) and with (b-d) pre-oxidation treatment after exposure for 500 h to stagnant oxygen-saturated LBE at 550oC (Inset in Fig.9a shows the EDS of the corrosion products) |
|