预氧化处理对12Cr铁素体/马氏体钢耐Pb-Bi腐蚀性能的影响 |
| 潘霞, 张洋鹏, 董志宏, 陈胜虎, 姜海昌, 戎利建 |
|
Effect of Pre-Oxidation Treatment on the Corrosion Resistance in Stagnant Liquid Pb-Bi Eutectic of 12Cr Ferritic/Martensitic Steel |
| PAN Xia, ZHANG Yangpeng, DONG Zhihong, CHEN Shenghu, JIANG Haichang, RONG Lijian |
| 图6 未预氧化和预氧化的12Cr铁素体/马氏体钢样品在550℃经饱和氧LBE腐蚀500和1000 h后腐蚀层截面形貌的SEM-BSE像 |
| Fig.6 Cross-sectional SEM-BSE images of 12Cr ferritic/martensitic steel samples without (a, b) and with (c, d) pre-oxidation treatment after exposure for 500 h (a, c) and 1000 h (b, d) to stagnant oxygen-saturated LBE at 550oC (Insets in Figs.6a and c show the high magnified images of oxide scale zone. IOZ—internal oxidation zone) |
|