预氧化处理对12Cr铁素体/马氏体钢耐Pb-Bi腐蚀性能的影响 |
| 潘霞, 张洋鹏, 董志宏, 陈胜虎, 姜海昌, 戎利建 |
|
Effect of Pre-Oxidation Treatment on the Corrosion Resistance in Stagnant Liquid Pb-Bi Eutectic of 12Cr Ferritic/Martensitic Steel |
| PAN Xia, ZHANG Yangpeng, DONG Zhihong, CHEN Shenghu, JIANG Haichang, RONG Lijian |
| 图1 高真空电阻炉示意图 |
| Fig.1 Schematic of the high vacuum resistance furnace |
|