超音速微粒轰击诱导表面纳米化对300M钢腐蚀疲劳行为的影响 |
| 熊毅, 栾泽伟, 马云飞, 厉勇, 查小琴 |
|
Effect of Surface Nanocrystallization Induced by Supersonic Fine Particles Bombardment on Corrosion Fatigue Behavior of 300M Steel |
| XIONG Yi, LUAN Zewei, MA Yunfei, LI Yong, ZHA Xiaoqin |
| 图9 SFPB处理300M钢不同载荷下腐蚀疲劳后微观组织的TEM像 |
| Fig.9 TEM images of SFPB-treated 300M steel after corrosion fatigue at different loads (a, b) topmost surface, σmax = 400 MPa (c, d) topmost surface, σmax = 800 MPa (Insets of Figs.9a and c show the SAED patterns, and insets in Figs.9b and d present the grain size distribution histograms calculated by Nano Measurer software) (e) subsurface, σmax = 400 MPa (f) subsurface, σmax = 800 MPa |
|