超音速微粒轰击诱导表面纳米化对300M钢腐蚀疲劳行为的影响 |
| 熊毅, 栾泽伟, 马云飞, 厉勇, 查小琴 |
|
Effect of Surface Nanocrystallization Induced by Supersonic Fine Particles Bombardment on Corrosion Fatigue Behavior of 300M Steel |
| XIONG Yi, LUAN Zewei, MA Yunfei, LI Yong, ZHA Xiaoqin |
| 图7 SFPB处理前后300M钢腐蚀疲劳后的表面形貌、表面粗糙度以及三维轮廓图(σmax = 400 MPa) |
| Fig.7 Surface morphologies (a, b), roughnesses Sa (c, d), and three-dimensional contour maps (e, f) of 300M steel without (a, c, e) and with (b, d, f) SFPB treatment after corrosion fatigue (σmax = 400 MPa) |
|