700℃时效对9Cr ODS钢微观组织和力学性能的影响 |
| 汪建强, 刘威峰, 刘生, 徐斌, 孙明月, 李殿中 |
|
Effect of Aging Treatment at 700oC on Microstructure and Mechanical Properties of 9Cr ODS Steel |
| WANG Jianqiang, LIU Weifeng, LIU Sheng, XU Bin, SUN Mingyue, LI Dianzhong |
| 图4 9Cr ODS钢在700℃时效1000 h的STEM像、相应的EDS面扫描图及颗粒A的SAED花样 |
| Fig.4 STEM image (a) and EDS mappings (b) of 9Cr ODS steel aged at 700oC for 1000 h, and SAED pattern of particle A in Fig.4a (c) |
|