取向硅钢不同常化工艺下组织及抑制剂的变化 |
| 杨伟阳, 黎先浩, 赵鹏飞, 于海彬, 赵松山, 罗海文 |
|
Changes in the Microstructures and Inhibitors of Grain-Oriented Silicon Steel Under Different Normalizing Processes |
| YANG Weiyang, LI Xianhao, ZHAO Pengfei, YU Haibin, ZHAO Songshan, LUO Haiwen |
| 图8 取向硅钢常化工艺中不同相变温度、时间和冷速下抑制剂形貌、平均尺寸与数量密度,及尺寸分布 |
| Fig.8 TEM images of inhibitors formed in P900-1 (a), P900-2 (b), P950 (c), and P900-2A (d) samples; corresponding average size and number density (e) and size distributions (f) |
|