取向硅钢不同常化工艺下组织及抑制剂的变化 |
| 杨伟阳, 黎先浩, 赵鹏飞, 于海彬, 赵松山, 罗海文 |
|
Changes in the Microstructures and Inhibitors of Grain-Oriented Silicon Steel Under Different Normalizing Processes |
| YANG Weiyang, LI Xianhao, ZHAO Pengfei, YU Haibin, ZHAO Songshan, LUO Haiwen |
| 图7 取向硅钢常化工艺中不同固溶温度下抑制剂的形貌、平均尺寸与数量密度,及尺寸分布 |
| Fig.7 TEM images of inhibitors formed in S950 (a), S1000 (b), S1120 (c), and S1200 (d) samples; corresponding average size and number density (e), and size distributions (f) |
|