取向硅钢不同常化工艺下组织及抑制剂的变化 |
| 杨伟阳, 黎先浩, 赵鹏飞, 于海彬, 赵松山, 罗海文 |
|
Changes in the Microstructures and Inhibitors of Grain-Oriented Silicon Steel Under Different Normalizing Processes |
| YANG Weiyang, LI Xianhao, ZHAO Pengfei, YU Haibin, ZHAO Songshan, LUO Haiwen |
| 图6 取向硅钢常化工艺中不同升温速率下抑制剂的形貌、成分、平均尺寸与数量密度,及尺寸分布 |
| Fig.6 TEM images of inhibitors formed in H2 (a), H10 (b), and H50 (c, d) samples; corresponding EDS (e-g), average size and number density (h) and size distribution (i) |
|