取向硅钢不同常化工艺下组织及抑制剂的变化 |
| 杨伟阳, 黎先浩, 赵鹏飞, 于海彬, 赵松山, 罗海文 |
|
Changes in the Microstructures and Inhibitors of Grain-Oriented Silicon Steel Under Different Normalizing Processes |
| YANG Weiyang, LI Xianhao, ZHAO Pengfei, YU Haibin, ZHAO Songshan, LUO Haiwen |
| 图4 不同常化工艺下取向硅钢的热膨胀曲线 |
| Fig.4 Dilatometric changes of grain-oriented silicon steel measured during the different normalizing processes (a, b) recorded dilations of S950, S1120, and S1200 samples varying with temperature (a) and time (b) (c) recorded dilation of P950 sample varying with time (Inset shows the locally enlarged curve) (d) recorded dilation of P900-2 varying with time (Inset shows the locally enlarged curve) |
|