取向硅钢不同常化工艺下组织及抑制剂的变化 |
| 杨伟阳, 黎先浩, 赵鹏飞, 于海彬, 赵松山, 罗海文 |
|
Changes in the Microstructures and Inhibitors of Grain-Oriented Silicon Steel Under Different Normalizing Processes |
| YANG Weiyang, LI Xianhao, ZHAO Pengfei, YU Haibin, ZHAO Songshan, LUO Haiwen |
| 图3 不同常化工艺下取向硅钢显微组织的SEM像及残余奥氏体的EBSD质量图和相图叠加图 |
| Fig.3 SEM images of grain-oriented silicon steel after the different normalizing processes (a-g) and EBSD quality map overlapped with phase map of retained austenite (h, i) (M—martensite) (a, h) S950 (b) S1000 (c) S1120 (d) S1200 (e, i) P900-2 (f) P950 (g) P900-2A |
|