全高丰度稀土(Ce, La, Y)-Fe-B永磁的研究现状和未来发展 |
| 刘仲武, 周帮, 廖雪峰, 何家毅 |
|
Research Status and Future Development of (Ce, La, Y)-Fe-B Permanent Magnets Based on Full High-Abundance Rare Earth Elements |
| LIU Zhongwu, ZHOU Bang, LIAO Xuefeng, HE Jiayi |
| 图9 Ce-Fe-B、(Ce, La)-Fe-B和(Ce, La, Y)-Fe-B热变形磁体的磁滞回线、微观结构[ |
| Fig.9 Hysteresis loops measured parallel (//) to the pressing direction of hot-deformed Ce17Fe78B6, (Ce0.9La0.1)Fe78B6, and [(Ce0.9La0.1)0.8Y0.2)]17Fe78B6 magnets (Inset shows the demagnetization curves of the hot-deformed magnets) (a), bright field TEM images of hot-deformed Ce17Fe78B6 (b) and [(Ce0.9La0.1)0.8Y0.2)]17Fe78B6 magnets (Insets show the HRTEM images of the hot-deformed magnets) (c), EDS line-scan profiles for hot-deformed Ce17Fe78B6 magnet (d)[ |
|