全高丰度稀土(Ce, La, Y)-Fe-B永磁的研究现状和未来发展 |
| 刘仲武, 周帮, 廖雪峰, 何家毅 |
|
Research Status and Future Development of (Ce, La, Y)-Fe-B Permanent Magnets Based on Full High-Abundance Rare Earth Elements |
| LIU Zhongwu, ZHOU Bang, LIAO Xuefeng, HE Jiayi |
| 图6 (Ce1 - x La x )Fe2相的形成能、(Ce1 - x La x )17Fe78B6快淬合金的XRD精修图谱[ |
| Fig.6 Calculated formation energiesfor (Ce1 - x La x )Fe2 phase (Inset shows the schematic illustration of the cubic CeFe2 crystal) (a), XRD refinement spectra for (Ce1 - x La x )17Fe78B6 alloys[ |
|