金属3D打印数字化制造研究进展
刘壮壮, 丁明路, 谢建新

Advancements in Digital Manufacturing for Metal 3D Printing
LIU Zhuangzhuang, DING Minglu, XIE Jianxin
图2 工业相机监测L-PBF粉末床铺粉质量(绿色表示零件轮廓,其他颜色代表不同缺陷)[48]
Fig.2 Industrial camera monitoring powder bed spreading quality in L-PBF (Green represents part outline, other colors indicate various defects)[48]