金属3D打印数字化制造研究进展 |
刘壮壮, 丁明路, 谢建新 |
Advancements in Digital Manufacturing for Metal 3D Printing |
LIU Zhuangzhuang, DING Minglu, XIE Jianxin |
图3 L-PBF成型仓内安装的激光轮廓仪示意图[ |
Fig.3 Schematic of profilometer installed inside L-PBF building chamber[ |
![]() |