金属圆棒超声螺旋扫查检测的合成孔径成像技术
|
|
李振杰, 蔡桂喜, 张博, 李经明, 李建奎
|
Synthetic Aperture Imaging Technology for Ultrasonic Spiral Scanning Detection of Metal Bars
|
|
LI Zhenjie, CAI Guixi, ZHANG Bo, LI Jingming, LI Jiankui
|
|
表1 人工缺陷位置及尺寸测量
|
Table 1 Location and size measurement of artificial defects
|
|
| Hole | Defect size | Defect position |
|---|
| number | ϕ / mm | ρ / mm | α / (º) | | Design value | Measured value | Absolute error | Design value | Measured value | Absolute error | Design value | Measured value | Absolute error | | 1# | 2.0 | 2.0 | 0 | 10.0 | 11.1 | 1.1 | 51 | 53 | 2 | | 2# | 2.0 | 2.0 | 0 | 10.0 | 10.8 | 0.8 | 74 | 72 | 2 | | 3# | 2.0 | 2.0 | 0 | 22.5 | 23.1 | 0.6 | 141 | 141 | 0 | | 4# | 2.0 | 2.0 | 0 | 22.5 | 23.8 | 1.3 | 151 | 151 | 0 | | 5# | 2.0 | 2.0 | 0 | 22.5 | 23.5 | 1.0 | 164 | 165 | 1 | | 6# | 1.0 | 1.4 | 0.4 | 22.5 | 23.7 | 1.2 | 235 | 234 | 1 | | 7# | 1.5 | 1.8 | 0.3 | 22.5 | 24.2 | 1.7 | 244 | 243 | 1 | | 8# | 2.0 | 2.0 | 0 | 22.5 | 24.6 | 2.1 | 254 | 255 | 1 | | 9# | 2.0 | 2.0 | 0 | 18.5 | 20.3 | 1.8 | 274 | 274 | 0 | | 10# | 2.0 | 1.8 | 0.2 | 14.5 | 15.9 | 1.4 | 294 | 295 | 1 | | 11# | 2.0 | 2.0 | 0 | 10.5 | 11.5 | 1.0 | 314 | 314 | 0 |
|
|
|