金属圆棒超声螺旋扫查检测的合成孔径成像技术 |
| 李振杰, 蔡桂喜, 张博, 李经明, 李建奎 |
|
Synthetic Aperture Imaging Technology for Ultrasonic Spiral Scanning Detection of Metal Bars |
| LI Zhenjie, CAI Guixi, ZHANG Bo, LI Jingming, LI Jiankui |
| 图9 ST-SAFT处理后的分辨率曲线 |
| Fig.9 Resolution curve after ST-SAFT processing |
|