金属圆棒超声螺旋扫查检测的合成孔径成像技术 |
| 李振杰, 蔡桂喜, 张博, 李经明, 李建奎 |
|
Synthetic Aperture Imaging Technology for Ultrasonic Spiral Scanning Detection of Metal Bars |
| LI Zhenjie, CAI Guixi, ZHANG Bo, LI Jingming, LI Jiankui |
| 图6 某一周扫查结果成像图 |
| Fig.6 Imaging charts of scanning results in a circle (a) B-scan image (b) cross-sectional image with raw data |
|