金属圆棒超声螺旋扫查检测的合成孔径成像技术 |
| 李振杰, 蔡桂喜, 张博, 李经明, 李建奎 |
|
Synthetic Aperture Imaging Technology for Ultrasonic Spiral Scanning Detection of Metal Bars |
| LI Zhenjie, CAI Guixi, ZHANG Bo, LI Jingming, LI Jiankui |
| 图5 钢制试样示意图 |
| Fig.5 Schematic diagram of steel specimen (ϕ—diameter of the specimen) (a) transverse-hole artificial defect sample (b) polar diagram of each transverse hole position |
|