表1 纯Ti α和β相的晶格常数(a、c)与实验值和其他理论值的比较[20~24]
Table 1 Lattice parameters (a, c) of the α and β phases of pure Ti in comparison with available values from experimental measurements and other theoretical calculations[20~24]
PhaseMethoda / nmc / a

α

EMTO0.29331.611
VASP[20]0.29241.595
VASP[21]0.29311.584
VASP[22]0.29461.584
Exp.[23]0.29511.585
βEMTO0.3261-
VASP[20]0.3252-
VASP[22]0.3264-
Exp.[24]0.3281-