第一性原理研究钛合金中的沉淀强化 |
| 程坤, 陈树明, 曹烁, 刘建荣, 马英杰, 范群波, 程兴旺, 杨锐, 胡青苗 |
|
Precipitation Strengthening in Titanium Alloys from First Principles Investigation |
| CHENG Kun, CHEN Shuming, CAO Shuo, LIU Jianrong, MA Yingjie, FAN Qunbo, CHENG Xingwang, YANG Rui, HU Qingmiao |
| 图5 Ti-Al-V合金α相和β相剪切模量EMTO-CPA计算值(灰色方柱)以及该计算值与采用模量Mo当量方法的估算值的绝对误差(青色方柱) |
| Fig.5 Shear moduli of α phase (a) and β phase (b) of Ti-Al-V alloy from direct EMTO-CPA calculations (gray column) and the error of the shear modulus evaluated with modulus Mo-equivalency (cyan column) |
|