第一性原理研究钛合金中的沉淀强化 |
| 程坤, 陈树明, 曹烁, 刘建荣, 马英杰, 范群波, 程兴旺, 杨锐, 胡青苗 |
|
Precipitation Strengthening in Titanium Alloys from First Principles Investigation |
| CHENG Kun, CHEN Shuming, CAO Shuo, LIU Jianrong, MA Yingjie, FAN Qunbo, CHENG Xingwang, YANG Rui, HU Qingmiao |
| 图4 二元钛合金Ti-xM (M = Al、V、Cr、Mn、Fe、Co、Ni、Zr、Nb、Mo、Ta、W)的β相多晶弹性模量随x的变化 |
| Fig.4 Polycrystalline elastic moduli of the β phase of binary Ti-xM (M = Al, V, Cr, Mn, Fe, Co, Ni, Zr, Nb, Mo, Ta, W) against x (a) bulk modulus (b) shear modulus (c) Young's modulus |
|