第一性原理研究钛合金中的沉淀强化 |
| 程坤, 陈树明, 曹烁, 刘建荣, 马英杰, 范群波, 程兴旺, 杨锐, 胡青苗 |
|
Precipitation Strengthening in Titanium Alloys from First Principles Investigation |
| CHENG Kun, CHEN Shuming, CAO Shuo, LIU Jianrong, MA Yingjie, FAN Qunbo, CHENG Xingwang, YANG Rui, HU Qingmiao |
| 图1 基体内均匀分布的球形沉淀相示意图 |
| Fig.1 Schematic representation of the spherical precipitation particle distributed homogenously in the matrix (R—radius of precipitate, L—spacing between precipitation phase particles) |
|