锂离子电池用微米厚度超薄集流体Cu箔和Al箔疲劳强度及损伤行为 |
| 程福来, 罗雪梅, 胡炳利, 张滨, 张广平 |
|
Fatigue Strength and Damage Behavior of Micron-Thick Ultrathin Current Collector Cu Foil and Al Foil for Lithium-Ion Battery |
| CHENG Fulai, LUO Xuemei, HU Bingli, ZHANG Bin, ZHANG Guangping |
| 图10 极值统计法预测最大缺陷尺寸 |
| Fig.10 Extreme value statistics predicting maximum defect size (a) linear fitting for parameters of Gumbel function for Al foils with different thicknesses ( (b) prediction of the maximum defect size under 95% probability |
|