高Nb锆合金在含氧蒸汽中耐腐蚀性能恶化的机理
黄建松, 裴文, 徐诗彤, 白勇, 姚美意, 胡丽娟, 谢耀平, 周邦新

Degradation Mechanism on Corrosion Resistance of High Nb-Containing Zirconium Alloys in Oxygen-Containing Steam
HUANG Jiansong, PEI Wen, XU Shitong, BAI Yong, YAO Meiyi, HU Lijuan, XIE Yaoping, ZHOU Bangxin
图7 合金在400℃、10.3 MPa的300 μg/kg DO过热蒸汽中腐蚀42 d氧化膜截面显微组织HAADF像及对应元素的EDS面分布图
Fig.7 HAADF images and corresponding EDS mappings of the complete region (a), region 1 (b), and region 2 (c) of cross-sectional oxide film on the alloy corroded in superheated steam with 300 μg/kg DO at 400oC and 10.3 MPa for 42 d