高Nb锆合金在含氧蒸汽中耐腐蚀性能恶化的机理
黄建松, 裴文, 徐诗彤, 白勇, 姚美意, 胡丽娟, 谢耀平, 周邦新

Degradation Mechanism on Corrosion Resistance of High Nb-Containing Zirconium Alloys in Oxygen-Containing Steam
HUANG Jiansong, PEI Wen, XU Shitong, BAI Yong, YAO Meiyi, HU Lijuan, XIE Yaoping, ZHOU Bangxin
图6 图5b中所示的SPP1~SPP3第二相的HRTEM像及FFT分析
Fig.6 HRTEM images and FFT analyses (insets) of the SPPs marked in Fig.5b, including SPP1 (a-e), SPP2 (f-h), and SPP3 (i), wherein magnifications of regions B-E (b-e) and G, H (g, h)