强流脉冲电子束辐照对低压等离子喷涂 MCrAlY涂层组织与性能的影响 |
| 蔡杰, 高杰, 花银群, 叶云霞, 关庆丰, 张小锋 |
|
Effect of High-Current Pulsed Electron Beam Irradiation on Microstructure and Properties of MCrAlY Coating Prepared by Low-Pressure Plasma Spraying |
| CAI Jie, GAO Jie, HUA Yinqun, YE Yunxia, GUAN Qingfeng, ZHANG Xiaofeng |
| 图10 HCPEB改性前后NiCrAlY涂层的TGO生长动力学及其拟合线 |
| Fig.10 TGO growth kinetics (a) and fitting lines (b) of NiCrAlY coatings before and after HCPEB modification (Kp—growth rate of oxide film) |
|