强流脉冲电子束辐照对低压等离子喷涂 MCrAlY涂层组织与性能的影响 |
| 蔡杰, 高杰, 花银群, 叶云霞, 关庆丰, 张小锋 |
|
Effect of High-Current Pulsed Electron Beam Irradiation on Microstructure and Properties of MCrAlY Coating Prepared by Low-Pressure Plasma Spraying |
| CAI Jie, GAO Jie, HUA Yinqun, YE Yunxia, GUAN Qingfeng, ZHANG Xiaofeng |
| 图1 强流脉冲电子束(HCPEB)改性前后NiCrAlY涂层的XRD谱 |
| Fig.1 XRD spectra of NiCrAlY coatings before and after high-current pulsed electron beam (HCPEB) modification |
|