放电等离子烧结Ni20Cr-xAl合金的高温氧化行为 |
| 刘丞济, 孙文瑶, 陈明辉, 王福会 |
|
High-Temperature Oxidation Behavior of Spark Plasma Sintered Ni20Cr-xAl Alloys |
| LIU Chengji, SUN Wenyao, CHEN Minghui, WANG Fuhui |
| 图9 铸态Ni20Cr-xAl合金在900℃恒温氧化100 h后局部截面的SEM像和元素面扫图 |
| Fig.9 Low and high (insets) magnified cross-sectional SEM images and corresponding element mapping of the as-cast Ni20Cr-xAl alloys with x = 1.5 (a), x = 3.0 (b), and x = 5.0 (c) after oxidation at 900oC for 100 h |
|