放电等离子烧结Ni20Cr-xAl合金的高温氧化行为 |
| 刘丞济, 孙文瑶, 陈明辉, 王福会 |
|
High-Temperature Oxidation Behavior of Spark Plasma Sintered Ni20Cr-xAl Alloys |
| LIU Chengji, SUN Wenyao, CHEN Minghui, WANG Fuhui |
| 图1 放电等离子烧结(SPS)制备Ni20Cr-xAl合金微观组织的SEM像 |
| Fig.1 SEM images of the Ni20Cr-xAl alloys with x = 1.5 (a), x = 3.0 (b), and x = 5.0 (c) prepared by spark plasma sintering (SPS) |
|