低温高应变量衬板控轧高固溶Al-Mg合金高强塑性与高热稳定性机制 |
| 田滕, 查敏, 殷皓亮, 花珍铭, 贾海龙, 王慧远 |
|
Enhanced Mechanical Properties and Thermal Stability Mechanism of a High Solid Solution Al-Mg Alloy Processed by Cryogenic High-Reduction Hard-Plate Rolling |
| TIAN Teng, ZHA Min, YIN Haoliang, HUA Zhenming, JIA Hailong, WANG Huiyuan |
| 图7 CHR-HPR Al-Mg合金经275℃退火30 min后微观组织的EBSD分析 |
| Fig.7 EBSD analyses of CHR-HPR Al-1Mg (a, d), Al-5Mg (b, e), and Al-9Mg (c, f) alloys annealed at 275oC for 30 min (ND—normal direction) (a-c) inverse pole figure maps (d-f) different types of grains |
|