低温高应变量衬板控轧高固溶Al-Mg合金高强塑性与高热稳定性机制 |
| 田滕, 查敏, 殷皓亮, 花珍铭, 贾海龙, 王慧远 |
|
Enhanced Mechanical Properties and Thermal Stability Mechanism of a High Solid Solution Al-Mg Alloy Processed by Cryogenic High-Reduction Hard-Plate Rolling |
| TIAN Teng, ZHA Min, YIN Haoliang, HUA Zhenming, JIA Hailong, WANG Huiyuan |
| 图1 挤压态和低温高应变量衬板控轧(CHR-HPR) Al-Mg合金的XRD谱 |
| Fig.1 XRD spectra of the as-extruded and cryogenic high-reduction hard-plate rolling (CHR-HPR) Al-Mg alloys (Dotted vertical lines represent the theoretical diffraction peaks of pure Al) |
|