Cr/Mo/W元素对镍基高温合金γ/γ′共格组织热稳定性的影响 |
| 凡莉花, 李金临, 孙九栋, 吕梦甜, 王清, 董闯 |
|
Effect of Cr/Mo/W on the Thermal Stability ofγ/γ′Coherent Microstructure in Ni-Based Superalloys |
| FAN Lihua, LI Jinlin, SUN Jiudong, LV Mengtian, WANG Qing, DONG Chuang |
| 图6 系列合金在900℃长期时效过程中γ /γ′共格组织演变 |
| Fig.6 Microstructure evolutions of the alloys S1-CM (a1-c1), S2-CW (a2-c2), and S3-CMW (a3-c3) aged at 900oC for 100 h (a1-a3), 200 h (b1-b3), and 500 h (c1-c3) |
|