连续屈服、高强屈比中锰钢的工艺设计与组织调控 |
| 张光莹, 李岩, 黄丽颖, 定巍 |
|
Process Design and Microstructure Control of Medium Manganese Steel with Continuous Yield and High Strength Yield Ratio |
| ZHANG Guangying, LI Yan, HUANG Liying, DING Wei |
| 图5 PA730-5试样拉伸断裂后距离断口不同位置的取样位置示意图及SEM像 |
| Fig.5 Schematic of sample location (a) and corresponding SEM images (b-d) away from fracture successively in PA730-5 sample |
|