Ag对奥氏体不锈钢组织和力学性能的影响 |
| 江浩文, 彭伟, 范增为, 汪杨鑫, 刘腾轼, 董瀚 |
|
Effect of Ag on Microstructure and Mechanical Properties of Austenitic Stainless Steel |
| JIANG Haowen, PENG Wei, FAN Zengwei, WANG Yangxin, LIU Tengshi, DONG Han |
| 图10 不同Ag含量不锈钢在{111}〈110〉滑移系下的晶粒Schmid因子分布 |
| Fig.10 Schmid factor distributions of grains in 304 (a), 304Ag-1 (b), and 304Ag-2 (c) stainless steels with different Ag contents under {111}〈110〉 slip systems |
|