Ag对奥氏体不锈钢组织和力学性能的影响 |
| 江浩文, 彭伟, 范增为, 汪杨鑫, 刘腾轼, 董瀚 |
|
Effect of Ag on Microstructure and Mechanical Properties of Austenitic Stainless Steel |
| JIANG Haowen, PENG Wei, FAN Zengwei, WANG Yangxin, LIU Tengshi, DONG Han |
| 图9 不同Ag含量不锈钢轧向(RD)、横向(TD)和法向(ND)的反极图 |
| Fig.9 Inverse pole figures of RD, TD, and ND of 304 (a), 304Ag-1 (b), and 304Ag-2 (c) stainless steels (ND—normal direction) |
|