Ag对奥氏体不锈钢组织和力学性能的影响 |
| 江浩文, 彭伟, 范增为, 汪杨鑫, 刘腾轼, 董瀚 |
|
Effect of Ag on Microstructure and Mechanical Properties of Austenitic Stainless Steel |
| JIANG Haowen, PENG Wei, FAN Zengwei, WANG Yangxin, LIU Tengshi, DONG Han |
| 图5 304Ag-2不锈钢的SEM像和EDS面扫描结果 |
| Fig.5 SEM image and corresponding EDS mappings of 304Ag-2 stainless steel |
|