Ag对奥氏体不锈钢组织和力学性能的影响 |
| 江浩文, 彭伟, 范增为, 汪杨鑫, 刘腾轼, 董瀚 |
|
Effect of Ag on Microstructure and Mechanical Properties of Austenitic Stainless Steel |
| JIANG Haowen, PENG Wei, FAN Zengwei, WANG Yangxin, LIU Tengshi, DONG Han |
| 图4 304Ag-1和304Ag-2不锈钢的SEM像 |
| Fig.4 SEM images of 304Ag-1 (a) and 304Ag-2 (b) stainless steels (Inset shows the high magnified image) |
|